●Mainly used in clothing label production or other types of silicone rubber products.
●Usage ratio: A : B=1000g:100g
●Take agent A, add appropriate amount of color paste, disperse evenly with a disperser, add a certain amount of agent B (it is recommended to be in the ratio of A:B= 10:1), mix evenly again and it is ready for use.
●When screen printing labels, the baking temperature is maintained at 100℃/10~60s. The specific conditions of vulcanization can also be determined by experiment according to the thickness or size of the product.
| Items | BQ-1033A/B |
| Appearance | Translucent without lumps A:6 million |
| Viscosity( mpa.s) | B :2000 |
| proportion(g/cm3) | 1.06-1.10 |
| Hardness (Shore A) | 35 |
| Tensile Strength(MPa) | ≥5 |
| Elongation(%) | ≥300 |
| Tear Strength(kN/m) | ≥15 |
| Operation time(25℃) | ≥4 |
● Store sealed in a cool, dry and ventilated place.
● The ambient temperature was maintained at 0-37°C.
Shelf life: 6 months.
Packing: A 20KG/barrel 200KG/barrel; B 1KG/can 20KG/barrel