Clean up the impurities of the item surface
Spray or soak or brush the primer onto the surface of the item
Bake it at temperature of 100℃ for 10 -15minutes
Molding it with silicone after drying. The adhesion is best after it is cool, do not peel both materials when it is still hot
Test item | Test condition and method | Result |
Appearance | Visual | Colorless to light yellow transparent liquid |
| Viscosity | Iwata 2# 25℃ | 7.5±0.5 S |
Effective solid content | 105℃,2h | 4%±0.5S |
Adhesion strength | Hand-stripping | 100% Cohesion damaged |
| Heat and cold impact | (80℃×1hr ~—40℃×1hr) ×12 recycle | No error |
Suitable for assembly joint of cell phone, laptop, household electrical appliances, ect electronics and other electronic device
Package: 1kg per can; 3kg per can
Storage: Stored in cool, dry and ventilated place at temperature of 0 to 35℃, humidity≤65%; Collection and storage it by galvanized metal, Polyethylene or polypropylene container; Stay far away from fire source
Shelf life: 3 months from production date, overdue material can be re- used after qualified.